MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo VYLOPET® CA3300 PC/PBT Polymer Alloy, Impact Resistant, Chemical Resistant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Applications:
  • Lamp parts
  • Home electric appliance parts
Features:
  • Fine appearance
  • Surface luster
  • Impact resistant
  • Chemical resistant

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Water Absorption 0.20 %24 hrs at 23°C; ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.00 mm
MD
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 3.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66.0 MPaASTM D638
Elongation at Break 140 %ASTM D638
Flexural Strength 96.0 MPaASTM D790
Flexural Modulus 2.60 GPaASTM D790
Izod Impact, Notched 82.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 °CMolding temperature
Mold Temperature 70.0 °C
Drying Temperature 130 °C
Dry Time 3 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant
A. Schulman Lucent PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade
A. Schulman Lucent PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade
A. Schulman Diamond DIAMALOY 527 PC/PBT Alloy

PTOY653 / 70813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.