MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® MP531201I Acrylate UV-Curing Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: MP531201I is a high performance UV curing adhesive engineered to bond plastics. It can be used in a variety of product assemblies and it promotes innovative design solutions. It is a fast cure, strong bonding adhesive. Our MP531201I is a leading performer when used for bonding general industrial applications. MP531201I is often cured with an electroless lamp D, medium pressure metal halide lamp. This UV adhesive also works well with UV light emitted diodes (UV LED) at wavelengths of 365 nm to 395 nm. Design engineers select MP531201I for the optimum in finished product quality, reliability, performance, and cost effectiveness. MP531201I is an essential tool in improving overall product quality, lowering per unit cost, and reducing processing time. Benefits: Superior Bond Strength, Solvent Free, Low Odor, Improves Finished Product Quality, Durable, Good Impact and Vibration Resistance, Easily Automated, No Clean Up. Substrate Applications: Polycarbonates, PET, PVC, Polyethylene, Polypropylene requires surface treatment, such as corona, etc.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³uncured
Water Absorption  0.70 %
@Temperature 100 °C,
Time 7200 sec
0.70 %
@Temperature 212 °F,
Time 2.00 hour
cured
 0.70 %
@Temperature 100 °C,
Time 86400 sec
0.70 %
@Temperature 212 °F,
Time 24.0 hour
cured
Viscosity 22000 - 37000 cP
@Temperature 25.0 °C
22000 - 37000 cP
@Temperature 77.0 °F
Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant <= 4.0<= 4.0cured
Dielectric Strength >= 15.7 kV/mm>= 400 kV/incured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 30.0 °C86.0 °Fcured
Flash Point 77.0 °C171 °Funcured
 
Descriptive Properties
Blue FluorescingNo. Cured
Chemical ClassAcrylate
Color / appearancegel
Flexible at Room Temperature?No
Water Resistance100% waterproof

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9121 / 233488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.