MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Braskem TN2005 EVA General Film Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility even at low temperatures and good sealing properties. TN2005 can be used as base polymer for the manufacture of films for greenhouses, with excellent thermal effect. It contains antioxidant additives. Its applications include: thermal agricultural film (greenhouse coverage) with no UV-additives, blown film mono or co-extrusion for food packaging, films for frozen food packaging, and high clarity film with excellent mechanical properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccASTM-D1505
Vinyl Acetate Content 13.5 %
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91ASTM-D2240
Hardness, Shore D 50ASTM-D2240
Tensile Strength at Break 25.0 MPaASTM-D638
Film Elongation at Break, MD 400 %ASTM-D882
Film Elongation at Break, TD 800 %ASTM-D882
Elongation at Break 680 %ASTM-D638
Secant Modulus, MD 0.600 GPa2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.700 GPa2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 100 gASTM-D1922
Elmendorf Tear Strength TD 270 gASTM-D1922
Elmendorf Tear Strength, MD 2.00 g/micronASTM-D1922
Elmendorf Tear Strength, TD 5.40 g/micronASTM-D1922
Dart Drop 8.50 g/micronASTM-D1709 (Method B)
Dart Drop Test 425 gASTM-D1709 (Method B)
Film Tensile Strength at Break, MD 30.0 MPaASTM-D882
Film Tensile Strength at Break, TD 34.0 MPaASTM-D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 94.0 °CASTM-D3418
Vicat Softening Point 75.0 °C
@Load 1.02 kg
ASTM-D1525
 
Optical PropertiesOriginal ValueComments
Haze 2.2 %ASTM-D1003
Gloss 82 %Angle 45°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.100 - 0.150 cmBlow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0Blow Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)170-185Blow Film Extrusion
Temperature Profile (°C)145-185Blow Film Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem CN8092 EVA Molding Copolymer
Braskem TN2006 EVA General Film Copolymer
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Braskem Evateno® 8019 PE EVA Foam Copolymer

PBRAS815 / 106661

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.