MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis HF700SA Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.600 g/cc
Density 0.905 g/ccISO 1183
Linear Mold Shrinkage 0.015 cm/cmmold average; Borealis Method
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ISO 2039-2
Ball Indentation Hardness 70.0 MPa358 N/30 s; ISO 2039
Tensile Strength, Yield 34.0 MPa50mm/min; ISO 527-2
Elongation at Yield 8.0 %50mm/min; ISO 527-2
Tensile Modulus 1500 MPa1mm/min; ISO 527-2
Charpy Impact Unnotched 15.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 3.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °C
@Thickness 2.00 mm
EN 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CISO 75-2
Vicat Softening Point 90.0 °C
@Load 5.10 kg
ISO 306
 153 °C
@Load 1.02 kg
ISO 306
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 120 °CUL 746B
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 3.00 mm
 
Optical PropertiesOriginal ValueComments
Gloss 70 %2mm plaque; DIN 67530
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 - 80.0 °C
Melt Temperature 220 - 260 °Cmass temperature
Mold Temperature 30.0 - 50.0 °C
Injection Velocity 100 - 200 mm/sec
Hold Pressure 30.0 - 60.0 MPa
 
Descriptive Properties
Back Pressurelow to medium
Screw Speedlow to medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® N 2320 003 UNC Q600 POM
Borealis HG313MO Polypropylene
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene
Borealis HH315MO Polypropylene
Borealis RF365MO Polypropylene

PBOREA488 / 108747

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.