MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Compounds Tehnamid® A-SV-35-2TM Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: 35% glass filled heat stabilized polyamide 66.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³GOST 15139
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
GOST 4650
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inGOST 18616
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm0.010 - 0.012 in/inGOST 18616
Melt Flow 7.0 - 15 g/10 min
@Load 2.16 kg,
Temperature 275 °C
7.0 - 15 g/10 min
@Load 4.76 lb,
Temperature 527 °F
GOST 11645
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 175 MPa25400 psiGOST 11262
Elongation at Break 4.0 %4.0 %GOST 11262
Flexural Strength 240 MPa34800 psiat maximum load; GOST 4648
Flexural Modulus 8.50 GPa1230 ksiGOST 9550
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -40.0 °C
26.2 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmGOST 6433.2
Dielectric Strength 35.0 kV/mm889 kV/inGOST 6433.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FGOST 15173
Melting Point 260 °C500 °FGOST 21553
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FGOST 12021
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FGOST 12021

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC127 / 307199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.