MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering V76E Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: ETP polymer. This peroxide cured compound is based on a tetrapolymer of Ethylene, Tetrafluoroethylene (TFE) and Perfluoromethylvinylether (PMVE), and a cure site monomer – 70-80 °IRHD.

Applications: This compound offers a higher level of fluid resistance than that of fluoroelastomers. It is not totally perfluorinated, so will not exhibit the ultra-low volume swell associated with Perlast® perfluoroelastomers. It is particularly suited to applications which have contact with strong amines, bases, steam and polar solvents. It improves on the chemical resistance of Aflas® and FKM elastomers, while retaining excellent low temperature performance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575°IRHD; ASTM D1415
Tensile Strength, Yield 18.4 MPa2670 psiASTM D412
Elongation at Break 180 %180 %ASTM D412
Compression Set 20 %
@Temperature 200 °C,
Time 86400 sec
20 %
@Temperature 392 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 206 °C403 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flash Point >= 315 °C>= 599 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Precision Polymer Engineering V85C Fluoroelastomer Compound
Precision Polymer Engineering V75I Fluoroelastomer Compound
Syensqo (Solvay Specialty Polymers) Tecnoflon® TN 80 Terpolymer Fluoroelastomer, Non-curative
ZEON Nipol® 1094-80 Nitrile Elastomer

PPRECI115 / 57839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.