MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LD 22014.BA Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 22014.BA resin is an easy flowing LDPE grade with good flexibility and excellent toughness.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Caps
  • Closures
  • Compounding
  • Food Packaging Containers
  • Houseware Articles
  • Injection Molding
  • Masterbatch Base Resin
  • Toys
  • Viscosity Modifier

Information provided by ExxonMobil

Key Words: LDPE LD 650
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 g/ccExxonMobil method
Melt Flow 22 g/10 min190°C/2.16kg; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4115sec; ISO 868
Tensile Strength at Break 1200 psiISO 527-2/1A/50
Elongation at Break 160 %ISO 527-2/1A/50
Tensile Modulus 17000 psiISO 527-2/1A/1
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 217 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 174 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 70013.BA Low Density Polyethylene Resin (European Grade)
LyondellBasell Lucalen A2920M Low Density Polyethylene
Celanese 191A LDPE polymer for adhesives, automotive and compounds
ExxonMobil EXACT™ 4150 Plastomer
ExxonMobil HD 5404 High Density Polyethylene Resin

PEX99285 / 175521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.