MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOLOR® PBT WT5065-17 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Base Polymer: Polybutylene Terephthalate

Color: White, similar to RAL 9010

Thermal Stability Colorant: 300°C max

Light Fastness Colorant: blue woolscale 8

For use in: Polyamide 6

Special Features: Free from cadmium, lead and diarylide pigments, dust-free, high dispersibility, high additive content

Market Segment: Electrical and Electronic, Furniture, Building and Construction, Sport and Leisure

Application Area: Injection molded parts, blow molded parts, extruded parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °CThermal Stability Colorant
Melt Temperature 250 - 270 °CInjection molding
Mold Temperature 60.0 - 100 °CInjection molding
Drying Temperature 100 - 120 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 100 - 120 °C
@Time 14400 - 28800 sec
in an circulating dryer
 
Descriptive Properties
Base PolymerPolybutylene Terephthalate
ColorWhite
Dosage (%)2extrusion
 2injection molded
Light Fastness Colorantblue woolscale 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® CFX PBT 1000 16072 PBT
Mocom (ALBIS) ALTECH® PBT A 1000/100 PBT
Arkema Platamid® H 2519 Pellets Polyamide
Mocom (ALBIS) ALCOLOR® PA A BL925-2287 Nylon 6
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow

PALBIS8408 / 242467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.