MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® X7167 Flame Retardant Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Flame Retardant

Material Notes: Description: High-viscosity resin with flame retardant, free of halogen and phosphorus, UL 94-V0/V2, with processing aid

Applications: Profiles for interior trim in aircraft

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12, EFH,22-020
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Moisture Absorption at Equilibrium 0.60 %
@Thickness 1.00 mm,
Temperature 23.0 °C
50% R.H.; ISO 62
Water Absorption at Saturation 1.5 %
@Thickness 1.00 mm
ISO 62
Linear Mold Shrinkage 0.011 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.012 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 48.0 MPaISO 527-1/2
Elongation at Break >= 50 %ISO 527-1/2
Elongation at Yield 5.0 %ISO 527-1/2
Tensile Modulus 1.70 GPaISO 527-1/2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 28.0 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.038
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VTest Solution A, 50 drops; IEC 60112
 600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °CPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Vicat Softening Point 150 °C50N; ISO 306
 175 °C10N; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Platamid® H 005 Pellets Polyamide
Evonik Vestamid® X7166 Flame Retardant Nylon 12
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
RTP Company RTP 299 F X 125585 H Nylon 12 (PA); Flame Retardant - Halogen Free
EMS-Grivory Grilamid® L 20H FWA black 9225 PA12

PHULA64 / 47424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.