MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem F2523 LDPE Blown Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose packaging that requires good optical and mechanical properties. Recommended film thickness: 0.020-0.100mm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM-D792
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 230 %ASTM-D882
Film Elongation at Break, TD 930 %ASTM-D882
Elmendorf Tear Strength TD 110 gASTM-D1922
Elmendorf Tear Strength, TD 4.40 g/micronASTM-D1922
Dart Drop 2.40 g/micronASTM-D1709
Dart Drop Test 60.0 gASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPaASTM-D882
Film Tensile Strength at Break, TD 20.0 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %ASTM-D1003
Gloss 110 %Angle 60°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 1.8 - 3.0Blow Film Extrusion
 
Descriptive Properties
Temperature Profile (°C)120-170Blow Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem F0421 D LDPE Blown Film Extrusion Polyethylene
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene
LyondellBasell Alathon® L5906 High Density Polyethylene

PBRAS828 / 106674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.