MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Outokumpu 2205 Duplex Stainless Steel
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel

Material Notes: Duplex stainless combining high mechanical strength with good corrosion resistance.

Applications:

  • Pulp and paper industry
  • Desalination plants
  • Flue-gas cleaning
  • Cargo tanks and pipe systems in chemical tankers
  • Seawater systems
  • Firewalls and blast walls on offshore platforms
  • Bridges
  • Components for structural design
  • Storage tanks
  • Pressure vessels
  • Heat exchangers
  • Water heaters
  • Rotors, impellers and shafts

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4462; UNS S32205, UNS S31803; JIS SUS 329J3L
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 750 MPa109000 psiOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 540 MPa
@Temperature 250 °C
78300 psi
@Temperature 482 °F
EN min.; EN 10002-5
 550 MPa
@Temperature 200 °C
79800 psi
@Temperature 392 °F
EN min.; EN 10002-5
 570 MPa
@Temperature 150 °C
82700 psi
@Temperature 302 °F
EN min.; EN 10002-5
 590 MPa
@Temperature 100 °C
85600 psi
@Temperature 212 °F
EN min.; EN 10002-5
Tensile Strength, Yield  460 MPa
@Strain 0.2 %
66700 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 510 MPa
@Strain 0.2 %
74000 psi
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 300 MPa
@Strain 0.2 %,
Temperature 250 °C
43500 psi
@Strain 0.2 %,
Temperature 482 °F
EN min.; EN 10002-5
 315 MPa
@Strain 0.2 %,
Temperature 200 °C
45700 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 335 MPa
@Strain 0.2 %,
Temperature 150 °C
48600 psi
@Strain 0.2 %,
Temperature 302 °F
EN min.; EN 10002-5
 360 MPa
@Strain 0.2 %,
Temperature 100 °C
52200 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 35 %35 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 200 GPa29000 ksiRT
 172 GPa
@Temperature 400 °C
24900 ksi
@Temperature 752 °F
 180 GPa
@Temperature 300 °C
26100 ksi
@Temperature 572 °F
 186 GPa
@Temperature 200 °C
27000 ksi
@Temperature 392 °F
 194 GPa
@Temperature 100 °C
28100 ksi
@Temperature 212 °F
Poissons Ratio 0.300.30RT
Fatigue Strength  510 MPa
@# of Cycles 2.00e+6
74000 psi
@# of Cycles 2.00e+6
R=smin/smax=0.1;RT; 50% probability of failure
 767 MPa
@# of Cycles 2.00e+6
111000 psi
@# of Cycles 2.00e+6
R=smin/smax=0.1; F50
 497 MPa
@Strain 0.2 %
72100 psi
@Strain 0.2 %
R=smin/smax=0.1; 2 million cycles, F50
Shear Modulus 77.0 GPa11200 ksicalculated
Impact Test >= 60.0 J>= 44.3 ft-lbEN 10045-1
 >= 40.0 J
@Temperature -40.0 °C
>= 29.5 ft-lb
@Temperature -40.0 °F
EN 10045-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm0.0000800 ohm-cmRT
 0.0000850 ohm-cm
@Temperature 100 °C
0.0000850 ohm-cm
@Temperature 212 °F
 0.0000900 ohm-cm
@Temperature 200 °C
0.0000900 ohm-cm
@Temperature 392 °F
 0.000100 ohm-cm
@Temperature 300 °C
0.000100 ohm-cm
@Temperature 572 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature 100 °C
7.22 µin/in-°F
@Temperature 212 °F
 14.5 µm/m-°C
@Temperature 400 °C
8.06 µin/in-°F
@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°FRT
 0.530 J/g-°C
@Temperature 100 °C
0.127 BTU/lb-°F
@Temperature 212 °F
 0.560 J/g-°C
@Temperature 200 °C
0.134 BTU/lb-°F
@Temperature 392 °F
 0.590 J/g-°C
@Temperature 300 °C
0.141 BTU/lb-°F
@Temperature 572 °F
Thermal Conductivity 15.0 W/m-K104 BTU-in/hr-ft²-°FRT
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 17.0 W/m-K
@Temperature 200 °C
118 BTU-in/hr-ft²-°F
@Temperature 392 °F
 18.0 W/m-K
@Temperature 300 °C
125 BTU-in/hr-ft²-°F
@Temperature 572 °F
 20.0 W/m-K
@Temperature 400 °C
139 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 1020 - 1100 °C1870 - 2010 °FQuench Annealing
 1020 - 1100 °C1870 - 2010 °FStress Relief Annealing
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 22 %22 %
Iron, Fe 69.01 %69.01 %
Molybdenum, Mo 3.1 %3.1 %
Nickel, Ni 5.7 %5.7 %
Nitrogen, N 0.17 %0.17 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 2205 Duplex Stainless steel
Carlson 2205 (UNS S31803) Duplex Stainless Steel
Carlson 2205 (UNS S32205) Duplex Stainless Steel
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34

NOUTOK06 / 18721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.