MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Categories: Ceramic; Carbide

Material Notes: Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties for ceramic fibers, and retains its properties at high temperatures. Nicalon™ is highly resistant to oxidation and chemical attack.

Product Forms:
Continuous Fiber: Supplied as multi-filament tow, spooled on 3 inch ID bobbins to 500 meters in length (100 grams in weight). Also available in random lengths at a reduced price.
Woven Cloth: Available in three weave styles as shown in Table 2. Woven cloth is typically supplied as 1-meter-wide continuous rolls of specific lengths. Other weave or braid styles can be made available.
Chopped Fiber: Available of 1-mm length chopped multi-filament tow. Longer lengths also available. Packaged as 3 kg containers.
Felt / Mat: Random lengths of Nicalon™ ceramic fiber in a PVA binder. Customizable areal weights, shapes and sizes.

Uses: Nicalon™ ceramic fiber can be used as a reinforcement for plastic, ceramic, and metal matrix composites to produce high performance composite materials. Surface treatments are normally recommended to facilitate processing and maximize composite properties Nicalon™ can also be used to form fibrous products such as high temperature insulation, filters, etc. Its resistance to chemical attack allows it to be used in harsh environments. The standard grade of the Nicalon™ product line; offers the optimum mechanical properties and high temperature performance for most applications.

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.55 g/cc0.0921 lb/in³
Filament Diameter 14 µm14 µm
Fiber Count 2000 dtex1800 denier
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3000 MPa435000 psi
Tensile Modulus 210 GPa30500 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cm
Dielectric Constant 9.29.2
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.20 µm/m-°C
@Temperature 25.0 - 500 °C
1.78 µin/in-°F
@Temperature 77.0 - 932 °F
 3.90 µm/m-°C
@Temperature 900 °C
2.17 µin/in-°F
@Temperature 1650 °F
Specific Heat Capacity  0.710 J/g-°C
@Temperature 25.0 °C
0.170 BTU/lb-°F
@Temperature 77.0 °F
 1.17 J/g-°C
@Temperature 500 °C
0.280 BTU/lb-°F
@Temperature 932 °F
Thermal Conductivity  2.20 W/m-K
@Temperature 500 °C
15.3 BTU-in/hr-ft²-°F
@Temperature 932 °F
 2.97 W/m-K
@Temperature 25.0 °C
20.6 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 32 %32 %
Oxygen, O 12 %12 %
Silicon, Si 57 %57 %
 
Descriptive Properties
Filaments per tow500

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Steatite (Magnesium Silicon Oxide)
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber
CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
Copper Tin Sulfide, Cu2SnS3

CCOIC012 / 122052

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.