MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A588 HSLA Steel Grade C, Thickness < 100 mm (4 in.)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel

Material Notes: HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM A588 has atmospheric corrosion resistance quadruple that of carbon steel. Used in welded, bolted, or riveted structures, especially bridges and buildings in which its strength and durability is required.

Key Words: UNS K11538
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 483 MPa>= 70000 psiVaries with size and form
Tensile Strength, Yield >= 345 MPa>= 50000 psiVaries with size and form
Elongation at Break >= 18 %>= 18 %in 200 mm (8 in.); Varies with size and form
 >= 21 %>= 21 %in 50 mm (2 in.); Varies with size and form
Modulus of Elasticity 205 GPa29700 ksiTypical of steel
Poissons Ratio 0.280.28Calculated
Shear Modulus 80.0 GPa11600 ksiTypical of steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 0.30 - 0.50 %0.30 - 0.50 %
Copper, Cu 0.20 - 0.50 %0.20 - 0.50 %
Iron, Fe 96.5 - 98.3 %96.5 - 98.3 %As Balance
Manganese, Mn 0.80 - 1.35 %0.80 - 1.35 %
Nickel, Ni 0.25 - 0.50 %0.25 - 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.050 %<= 0.050 %
Vanadium, V 0.010 - 0.10 %0.010 - 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A588 HSLA Steel Grade D, Thickness < 100 mm (4 in.)
ASTM A588 HSLA Steel Grade B, Thickness < 100 mm (4 in.)
ASTM A588 HSLA Steel Grade K, Thickness < 100 mm (4 in.)
ASTM A588 HSLA Steel Grade A, Thickness < 100 mm (4 in.)
ASTM A572 Steel, grade 60

MSA588C0 / 14030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.