MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of cast nylons may be altered to suit specific applications, and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colorants.

Key characteristics:

  • Unequalled formulation options and profile range
  • Excellent mechanical, thermal and chemical resistance
  • Excellent PV and load bearing capabilities
  • Excellent wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA compliant grades available

This grade was specifically developed for applications requiring high impact resistance. Other important characteristics are improved insensitivity against stresses, sharp edges, notches and scratches. It also exhibits improved noise reduction and great load bearing capabilities.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³Test Method A; ISO 1183:1987
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ISO 868:2003
Tensile Strength at Break 60.0 MPa8700 psiSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 30 %>= 30 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.20 GPa464 ksiSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 85.0 MPa12300 psi1.5 mm/min; ISO 178:2001
Flexural Modulus 2.40 GPa348 ksi1.5 mm/min; ISO 178:2001
Compressive Strength 90.0 MPa13100 psiSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 1.80 GPa261 ksiSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²Sample Type A; ISO 180:2000
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1:1998-01
Comparative Tracking Index 600 V600 VIEC 60112:2003-01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 200 °C392 °F
Maximum Service Temperature, Air 100 °C212 °FContinuous
 150 °C302 °FIntermittent
Minimum Service Temperature, Air -100 °C-148 °FIntermittent
 -40.0 °C-40.0 °FContinuous
Flammability, UL94 HBHBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade
LG Chemical LGflex GL300 Plasticizer
ExxonMobil Jayflex™ 210 Naphthenic Hydrocarbon Plasticizer
BASF Palamoll® 654 Polymeric Plasticizer
Avient reFlex™ 300 Plasticizer, Bio-derived

PGLOEPP07 / 79518

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.