MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 954-3 Curing Cyanate Resin, K1100 Fiber
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 1310 MPa
@Temperature 23.0 °C
190000 psi
@Temperature 73.4 °F
Tensile Modulus 565 GPa
@Temperature 23.0 °C
81900 ksi
@Temperature 73.4 °F
Compressive Yield Strength 269 MPa
@Temperature 23.0 °C
39000 psi
@Temperature 73.4 °F
Compressive Modulus 565 GPa
@Temperature 23.0 °C
81900 ksi
@Temperature 73.4 °F
Shear Strength 23.0 MPa
@Temperature 22.0 °C
3340 psi
@Temperature 71.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-2A Curing Cyanate Resin, K1100 Fiber
Solvay Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System
Overview of materials for Epoxy/Carbon Fiber Composite
Covestro Apec® 1695 Polycarbonate
Aluminum 1060-H14

PHEXC031 / 98501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.