MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zeon Specialty Materials ZEONOR® 1430R Cyclo Olefin Polymer
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: High flow, high transparency, low fluorescence grade for light guide and diagnostic consumable

Information provided by Zeon Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Melt Flow 30 g/10 min
@Load 2.18 kg,
Temperature 280 °C
30 g/10 min
@Load 4.81 lb,
Temperature 536 °F
JIS 6719
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiISO 527
Elongation at Break 16 %16 %ISO 527
Tensile Modulus 2.30 GPa334 ksiISO 527
Flexural Modulus 2.20 GPa319 ksiISO 178
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.3
@Frequency 1e+9 Hz
2.3
@Frequency 1e+9 Hz
ASTM D150
Dissipation Factor <= 0.0010
@Frequency 1e+9 Hz
<= 0.0010
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FASTM E831
Glass Transition Temp, Tg 136 °C277 °FJIS K7121
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 %
@Thickness 3.00 mm
92 %
@Thickness 0.118 in
ASTM 1003
 
Descriptive Properties
Colorclear
Featureshigh purity
Primary MarketLight Guide
Processing MethodBlow Molding
REACHYes
RoHSYes
UsesMirror

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zeon Specialty Materials ZEONOR® 1420R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1410R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1020R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1060R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 750R Cyclo Olefin Polymer

PZEONC82r / 191536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.