MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tensile strengths to be achieved by rolling with a lower loss of ductility. When this grade is cold worked it becomes more magnetic than other austenitic stainless steels. Typical uses include aircraft structural parts, diaphragms, utensils, automotive trim, and conveyor belts.

Information provided by Eagle Brass Company

Key Words: ASTM A666; UNS S30100
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³As Annealed
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 862 MPa>= 125000 psi
Tensile Strength, Yield >= 517 MPa>= 75000 psi0.2% Offset
Elongation at Break >= 25 %>= 25 %in 2 inches
Tensile Modulus 193 GPa28000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 649 °C
10.4 µin/in-°F
@Temperature 68.0 - 1200 °F
Thermal Conductivity 16.3 W/m-K113 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 74.775 - 78 %74.775 - 78 %Calculated as Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 6.0 - 8.0 %6.0 - 8.0 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened
Eagle Brass 301 Austenitic Stainless Steel, Annealed
Eagle Brass 301 Austenitic Stainless Steel, Full Hardened
301 Stainless Steel
Eagle Brass 301 Austenitic Stainless Steel, 3/4 Hardened

NEAGLE509 / 147489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.