MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ 165HB Urethane Coating
Categories: Polymer; Thermoset

Material Notes: 3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in many different immersion conditions, including sea, foul and raw water; also in chemically polluted, marine or underground environments. Scotchkote urethane coating 165HB is specifically designed for plural feed hot airless spray application. As such it permits single coat applications of between 0.5 mm and 2 mm dft.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Water Absorption 0.26 %0.26 %24 hrs; ASTM D570
 1.19 %1.19 %21 days; ASTM D570
Thickness 1020 microns40.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ASTM D2240
Tensile Strength at Break 14.3 MPa2070 psiASTM D638
Elongation at Break 24 %24 %ASTM D638
Impact Test 7.00 J5.16 ft-lb1/4" steel plate; ASTM G14 (modified)
Abrasion 9898[mg] loss per 1000 cycles; ASTM D4060
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °F
Minimum Service Temperature, Air 0.000 °C32.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourTouch Dry
 360 min6.00 hourHard Dry
 10100 min168 hourFull Cure
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblock® Base GS Acrylic Basecoat
Total 3181 Polypropylene, Extrusion Grade
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer

PMM35338 / 170085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.