MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 White Oil Premium Food-Grade Mineral Oil, Grade 50/60, ISO 7/10
Categories: Fluid; Lubricant

Material Notes: Phillips 66® White Oil is a highly refined, premium quality mineral oil developed for use in food processing plants, consumer products, and in other applications that require an exceptionally pure white mineral oil. It meets or exceeds the highest industry standards for purity and stability. All viscosity grades are registered by NSF International as H1 lubricants for use where incidental food contact may occur, and are certified Kosher and Pareve. They also are certified as meeting Canadian Food Inspection Agency requirements for use in federally registered food plants. White Oil is manufactured with hydro-processed base oils of the highest purity. It contains Vitamin E as a natural oxidation inhibitor and remains colorless, odorless, and tasteless during normal storage and service life. It is non-toxic and has outstanding storage stability. White Oil meets FDA requirements for use in applications where direct, indirect, or incidental contact with food may occur. It may be used to lubricate machinery, protect against moisture, or control dust on grains and animal feed. It also is used as a component in certain consumer products such as cosmetics and pharmaceuticals. The 340/365 grade also is registered as NSF 3H for use as a release agent to prevent sticking on grills, ovens, chopping boards, and other hard surfaces in contact with meat and poultry.

Applications:

  • Food processing, bottling and canning equipment
  • Protective coating for raw fruits and vegetables
  • Egg shell sealant in facilities operating under the USDA voluntary shell egg grading program
  • Non-stick release agent in meat and poultry plants
  • Dust suppressant for grain or animal feed
  • Drip oil for deep well water pumps
  • Process oil or diluent in adhesives, sealants, caulks, cosmetics, pharmaceuticals, rubber extender oils and plastics
  • Smoke oil for air shows
  • Textile lubricants
  • Household cleaners and polishes
White Oil meets the requirements of the following government and industry specifications:
  • Canadian Food Inspection Agency (CFIA) requirements for use in federally registered food plants (incidental food contact)
  • Cosmetic, Toiletry, and Fragrance Association (CTFA)
  • FDA Code of Federal Regulations: 21 CFR 172.878 for direct food contact and 21 CFR 178.3620 for indirect food contact
  • National Formulary (NF) (Grades 50/60, 65/75, 80/90)
  • NSF International H1 and former 1998 USDA H1 guidelines for incidental food contact (Registration Nos. 137240, 137241, 137242, 137243, 137244)
  • USDA voluntary shell egg grading program, for protective coating (Grades 50/60, 65/75 and 80/90)
  • United States Pharmacopoeia (USP) (Grades 200/215, 340/365)
Features/Benefits:
  • Colorless, odorless and tasteless
  • Excellent color stability
  • Contains Vitamin E for oxidation inhibition
  • Non-staining
  • Certified Kosher and Pareve

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.842 g/cc0.842 g/cc
Density 0.840 g/cc0.0303 lb/in³
Viscosity Measurement 8383Index
Saybolt Viscosity at 100°F 55 SUS55 SUS
Saybolt Viscosity at 210°F 34 SUS34 SUS
Kinematic Viscosity at 40°C (104°F) 8.3 cSt8.3 cSt
Kinematic Viscosity at 100°C (212°F) 2.3 cSt2.3 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -9.00 °C15.8 °F
Flash Point 174 °C345 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USDA YesYes
 
Descriptive Properties
Color30Saybolt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Superla® 50 White Oil
Phillips 66 White Oil Premium Food-Grade Mineral Oil, Grade 65/75, ISO 10/15
ChevronTexaco Packers Oil
Chesterton 662 FG Barrier Fluid 22
Anderol ANDEROL® PQ AA 85W140 White Mineral Food Grade Gear Oil, ISO Grade 320, SAE Gear Oil Grade 85W140

WCON5453 / 198706

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.