MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom HRG 328T NAT Polypropylene with 30% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Hostacom HRG 328T NAT is a 30% glass fiber reinforced PP homopolymer, with high flowability, very good stiffness, low CLTE (Coefficient of Linear Thermal Expansion), low creep under load at elevated temperatures and low emissions. The product is available as natural, pellet form. Applications: Automotive Parts

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183-1A
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527-1,-2
Elongation at Break 2.6 %2.6 %ISO 527-1,-2
Tensile Modulus 6.80 GPa986 ksiISO 527-1,-2
Flexural Strength 145 MPa21000 psiTech.A; ISO 178/A1
Flexural Modulus 7.20 GPa1040 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 135 °C275 °FB50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Fibremod™ GB366WG Polypropylene Compound, Glass Fiber Reinforced
LATI Latene® AG30H G/30 30% Glass Fiber, Chemically Coupled, Heat-Stabilized Polypropylene Homopolymer (PPH)
LyondellBasell Hostacom G3 R11 105290 Polypropylene with 30% Glass Fiber Filler
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized
LATI Latene® AG3H2W G/30-V0 30% Glass Fiber with Chemical Bond, Heat-Stabilized Polypropylene Homopolymer (PPH)

PEQT7996 / 219632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.