MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SunChemical Gwent C2060602D1 Membrane Touch Switch Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.
Can be used in membrane touch switch applications
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156 to 230tpi
Substrate: Polyester, PVC, or Ceramic.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 39 - 41 %
@Temperature 130 °C
39 - 41 %
@Temperature 266 °F
Viscosity 4000 - 6000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
4000 - 6000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 12 - 25 ohm
@Thickness 0.0250 mm
12 - 25 ohm
@Thickness 0.000984 in
Using a 2300 mesh stainless steel screen
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 80.0 °C
0.167 hour
@Temperature 176 °F
 30.0 min
@Temperature 60.0 °C
0.500 hour
@Temperature 140 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Coverage cm2/g288Using a 200 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® ELKONIUM® 40 pure palladium

WGELZ9035 / 139348

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.