MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Water Absorption 3.7 - 4.3 %3.7 - 4.3 %ISO 62
Moisture Absorption at Equilibrium 1.0 - 1.4 %1.0 - 1.4 %ISO 62
Viscosity Measurement 140140ISO 307
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/in
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0085 cm/cm0.0085 in/inISO 2577
Melt Flow 15.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
15.5 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357-1/-3
Maximum Service Temperature, Air 240 °C464 °F
Decomposition Temperature >= 310 °C>= 590 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 300 °C572 °FFeed zone
Zone 2 300 °C572 °FCompression
Zone 3 300 °C572 °FMetering-zone
Zone 4 300 °C572 °FNozzle
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding/Extrusion
 300 °C572 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection Molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 20560
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry)
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned)
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Conditioned)
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry)
BASF Ultramid® A3WG6 LS BK 23189 30% Glass Filled PA66 (Dry)

PBASG0366 / 131999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.