MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® SV-0167EX Extrusion Grade ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9999ASTM D785
Tensile Strength, Yield 40.0 MPa
@Thickness 3.17 mm
5800 psi
@Thickness 0.125 in
ASTM D638
Flexural Strength 57.9 MPa
@Thickness 3.17 mm
8400 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 1.93 GPa
@Thickness 3.17 mm
280 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 4.81 J/cm
@Thickness 3.17 mm
9.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 6.35 mm
194 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 99.0 °C210 °FUnannealed; ISO R 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 - 220 °C392 - 428 °F
Middle Barrel Temperature 220 - 240 °C428 - 464 °F
Front Barrel Temperature 230 - 250 °C446 - 482 °F
Nozzle Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.9 - 82.7 MPa10000 - 12000 psi
Back Pressure 0.689 - 1.38 MPa100 - 200 psi
Shot Size 50 - 80 %50 - 80 %
Screw Speed 30 - 60 rpm30 - 60 rpm
 
Descriptive Properties
Processing Fill SpeedSlow to Moderate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® SV-0167 ABS, Unreinforced Extrusion Grade
Lotte Advanced Materials Starex® SP-0183 ABS, Unreinforced Extrusion Grade
Lotte Advanced Materials Starex® SV-0165 U ABS, Unreinforced Extrusion Grade
LG Chemical HI100 ABS, High Impact
Asahi Kasei Stylac™ AE850 ABS Polymer, Extrusion, High Molding

PLBST004 / 50489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.