MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hours at 73°F; ASTM D570
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
22 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 60.3 MPa
@Thickness 3.17 mm
8750 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 120 %
@Thickness 3.17 mm
120 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 89.6 MPa
@Thickness 3.17 mm
13000 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.41 GPa
@Thickness 3.17 mm
350 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 7.47 J/cm
@Thickness 3.17 mm
14.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secPLC 6
Comparative Tracking Index 250 - 400 V250 - 400 VPLC 2
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness 1.50 mm
15 - 30 sec
@Thickness 0.0591 in
PLC 3
 30 - 60 sec
@Thickness 3.00 mm
30 - 60 sec
@Thickness 0.118 in
PLC 2
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
PLC 1
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
PLC 0
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.2 µm/m-°C
@Temperature -40.0 - 95.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831-06
CTE, linear, Transverse to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831-06
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °FASTM D648
 137 °C279 °FISO 75
UL RTI, Electrical 125 °C257 °F
UL RTI, Mechanical with Impact 115 °C239 °F
UL RTI, Mechanical without Impact 125 °C257 °F
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
Glow Wire Ignition Temperature 775 °C1430 °F
Glow Wire Flammability Index 960 °C1760 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.586
@Wavelength 589.3 nm
1.586
@Wavelength 589.3 nm
nD
Haze 1.0 %1.0 %
Transmission, Visible 89 %89 %
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 243 - 260 °C470 - 500 °F
Middle Barrel Temperature 249 - 260 °C480 - 500 °F
Front Barrel Temperature 260 - 271 °C500 - 520 °F
Nozzle Temperature 254 - 271 °C490 - 520 °F
Melt Temperature 260 - 282 °C500 - 540 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hour48 hours max.
Injection Pressure 51.7 - 124 MPa7500 - 18000 psi
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Clamp Pressure 27.6 - 68.9 MPa4000 - 10000 psi
Shot Size 40 - 60 %40 - 60 %
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow to Medium
Injection Speed- Tab GateMedium to Fast
Injection Speed- Tunnel GateFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release
Covestro Bayblend® T65 HG PC/ABS Blend
OGC OKP4 Polyester Optical Plastic
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber

PZ9PU12 / 21566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.