MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Sequel 2405 NAT Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Sequel 2405 NAT very high melt flow, very high modulus engineered polyolefin is typically used for large mold-in-color interior applications for the transportation industry that require stiffness, dimensional stability, and good impact characteristics. This material exhibits excellent processability and appearance for mold-in-color applications. Applications: Instrument Panels, Interior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Melt Flow 35 g/10 min35 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psi50mm/min; ISO 527-1,-2
Flexural Modulus 2.30 GPa334 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C243 °Funannealed; ISO 75B-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Sequel 2396 SP GP BLACK Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP YR400L Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP NH767L TRUFFLE GR Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP NH690L PREMIUM BLK Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP NH686L Thermoplastic Olefinic Elastomer

PEQT8768 / 220402

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.