MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Celstran® PA6-GF60-01 Nylon 6, 60% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: 60% long strand glass fiber reinforced nylon 6 Natural

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.69 g/cc1.69 g/ccASTM D792
Density 1.69 g/cc0.0611 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm0.00050 - 0.0010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 250 MPa36300 psi5mm/min; ISO 527-2/1A
 276 MPa40000 psiASTM D638
 134.4 MPa
@Temperature 121 °C
19490 psi
@Temperature 250 °F
ASTM D638
 328.6 MPa
@Temperature -40.0 °C
47660 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 1.58 %1.58 %5mm/min; ISO 527-2/1A
 1.9 %1.9 %ASTM D638
 2.0 %
@Temperature 121 °C
2.0 %
@Temperature 250 °F
ASTM D638
 2.1 %
@Temperature 4.44 °C
2.1 %
@Temperature 40.0 °F
ASTM D638
Tensile Modulus 20.3 GPa2940 ksi50mm/min; ISO 527-2/1A
 22.1 GPa3200 ksiASTM D638
 13.9 GPa
@Temperature 121 °C
2020 ksi
@Temperature 250 °F
ASTM D638
 21.7 GPa
@Temperature -40.0 °C
3150 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 405 MPa58700 psiISO 178
 429 MPa62200 psiASTM D790
 200.0 MPa
@Temperature 121 °C
29010 psi
@Temperature 250 °F
ASTM D790
 478.1 MPa
@Temperature -40.0 °C
69340 psi
@Temperature -40.0 °F
ASTM D790
Flexural Modulus 18.2 GPa2640 ksiISO 178
 18.6 GPa2700 ksiASTM D790
 9.51 GPa
@Temperature 121 °C
1380 ksi
@Temperature 250 °F
ASTM D790
 20.0 GPa
@Temperature -40.0 °C
2900 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 5.23 J/cm9.80 ft-lb/inASTM D256
 4.97 J/cm
@Temperature -40.0 °C
9.30 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 6.03 J/cm
@Temperature 121 °C
11.3 ft-lb/in
@Temperature 250 °F
ASTM D256
Charpy Impact, Notched 4.80 J/cm²22.8 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FASTM D648
 215 °C419 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 265 - 275 °C509 - 527 °F
Zone 2 270 - 275 °C518 - 527 °F
Zone 3 275 - 280 °C527 - 536 °F
Zone 4 275 - 280 °C527 - 536 °F
Die Temperature 275 - 280 °C527 - 536 °F
Melt Temperature 270 - 280 °C518 - 536 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.18 %<= 0.18 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade
LG Chemical LUMID HM2604AW PA6+GF60%
EMS-Grivory Grilamid® XE 4106 nat PA612-GF30
EMS-Grivory Grilon® BG-60 FC PA6-GF60
Celanese Zytel® 77G33L BK031 PA612-GF33

PHCQ186 / 178641

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.