MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Gapex® RPP30EB56BK 30% Fiberglass Reinforced, Chemically-Coupled, Heat Stabilized, Homopolymer Polypropylene containing 25% minimum P.C.R.
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: 30% Fiberglass Reinforced, Chemically-Coupled, Heat Stabilized, Homopolymer Polypropylene containing 25% minimum P.C.R.

Description: Precolored black

Applications: Primary use is for battery tray supports.

Specifications: Meets/exceeds Ford Engineering Material Specification WSS-M4D732-A5

Comments: Tensile/Izod Change (1000 hrs./140°C): +7/-12%; WSS-M4D732-A5 Specification: ±25/-25; ISO 188
Filler Content: 30.3% ;WSS-M4D732-A5 Specification: 28.0-32.0; ISO 3451/1A
Material Pre-dry: Normally it is not necessary to pre-dry this material. However, if conditions dictate drying to optimize material properties and part appearance then dry in a desiccant dryer at 180°F for 2-3 hours or 160°F for >4 hours.
Manifolds: Maintain manifolds, runners and tips 10 to 20°F above the front one temperature to allow easier filling. (Gate drool is best eliminated using screw decompression rather than reducing tip temperature.)
Back Pressure (Range): 20-50 psi. Injection Speed: medium to slow > depending on surface appearance. Screw Speed: medium. Injection Pressure: Adjust to just above a short shot. Injection Time: Adjust to just above a short shot. Cushion (Range): 0.2-0.5 in. Nozzle Type: Free flowing/Standard.
Some conditions may have to be altered to obtain acceptable parts. Please do not run too cold, molded in stress and rough surface may become a problem. If you must run below melt or temperatures recommended for dimensional precision you may compromise impact and esthetics. Retest parts to confirm performance.

Data provided by Ferro Corporation - Specialty Plastics Group.

A. Schulman has acquired the Ferro specialty plastics business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³WSS-M4D732-A5 Specification: 1.10-1.16 g/cc; ISO R 527
Linear Mold Shrinkage 0.0065 cm/cm0.0065 in/inISO 2577
Melt Flow 4.0 g/10 min4.0 g/10 minWSS-M4D732-A5 Specification: 2.0-6.0 g/10 min; ISO R 527
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 71.9 MPa10400 psiWSS-M4D732-A5 Specification: 68 MPa Min.; ISO R 527
Flexural Modulus 5.00 GPa725 ksiWSS-M4D732-A5 Specification: 4.3 GPa Min.; ISO R 527
Izod Impact, Notched (ISO) 6.80 kJ/m²3.24 ft-lb/in²WSS-M4D732-A5 Specification: 4.5 kJ/m² Min.; ISO R 527
 4.90 kJ/m²
@Temperature -40.0 °C
2.33 ft-lb/in²
@Temperature -40.0 °F
WSS-M4D732-A5 Specification: 3.5 kJ/m² Min.; ISO R 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FWSS-M4D732-A5 Specification: 145°C; ISO R 527
Deflection Temperature at 1.8 MPa (264 psi) 142 °C288 °FWSS-M4D732-A5 Specification: 130°C; ISO R 527
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 221 - 238 °C430 - 460 °F
Middle Barrel Temperature 227 - 243 °C440 - 470 °F
Front Barrel Temperature 232 - 260 °C450 - 500 °F
Nozzle Temperature 232 - 260 °C450 - 500 °F
Mold Temperature 37.8 - 60.0 °C100 - 140 °FCore. Cooler temperatures may be needed to maintain dimensions or eliminate sinks in thick sections.
 43.3 - 65.6 °C110 - 150 °FCavity
Drying Temperature 82.2 °C180 °F2-3 hrs at 180°F or 4+ hours at 160°F.
Dry Time 2 - 3 hour2 - 3 hour
 
Descriptive Properties
ColorPrecolored black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Gapex® RPP20EA11BK 20% Fiberglass Reinforced, Heat-Stabilized, Chemically-Coupled, Homopolymer Polypropylene
Entec Hypro™ F PPH-GF40 Natural Homopolymer Polypropylene, 40% Glass Reinforced
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized
A. Schulman Gapex® RPP30DA10BK 30% Fiberglass Reinforced, Heat Stabilized, Homopolymer Polypropylene
Birch Plastics RPP1215 Recycled Polypropylene

PFERRO45 / 38159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.