Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties:- Excellent flow behavior
- High toughness
- Very good surface finish
- Easy processing
Grilon TSS is used typically for various applications in the automotive, the electro and the sports & leisure field such as loudspeaker grids, interior casings, chair rollers, handles and levers. According to FDA (21 CFR 177.1500 and corresponding paragraphs covering the additives) GRILON TSS/2 FA is also approved for the direct contact with non-alcoholic foodstuffs.Information provided by EMS Grivory. |