System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
BASF Ultramid® A3ZG7 HP BK 20465 33% Glass Filled PA66 (Dry)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
Description: Ultramid A3ZG7 HP BK20465 is a 33% glass reinforced, heat stabilized, impact modified PA66 black with a combination of excellent impact resistance, toughness and strength.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.33
g/cc
0.0480
lb/in³
ISO 1183
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
140
MPa
20300
psi
ISO 527
Elongation at Break
4.8 %
4.8 %
ISO 527
Tensile Modulus
8.85
GPa
1280
ksi
ISO 527
Flexural Modulus
7.98
GPa
1160
ksi
ISO 178
Izod Impact, Notched (ISO)
17.0
kJ/m²
@Temperature -30.0 °C
8.09
ft-lb/in²
@Temperature -22.0 °F
ISO 180
24.0
kJ/m²
@Temperature 23.0 °C
11.4
ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched
1.80
J/cm²
@Temperature -30.0 °C
8.57
ft-lb/in²
@Temperature -22.0 °F
ISO 179
2.30
J/cm²
@Temperature 23.0 °C
10.9
ft-lb/in²
@Temperature 73.4 °F
ISO 179
Thermal Properties
Metric
English
Comments
Melting Point
260
°C
500
°F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi)
260
°C
500
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
244
°C
471
°F
ISO 75
Processing Properties
Metric
English
Comments
Melt Temperature
288
-
305
°C
550
-
581
°F
Mold Temperature
60.0
-
100
°C
140
-
212
°F
Dry Time
1
-
2
hour
1
-
2
hour
Injection Pressure
35.0
-
125
MPa
5080
-
18100
psi
Back Pressure
0.000
-
0.350
MPa
0.000
-
50.8
psi
Screw Speed
40
-
80
rpm
40
-
80
rpm
Descriptive Properties
Color
BK 20465
Commercial Status
North America
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3WG10 50% Glass Filled PA66 (Dry)
BASF Ultramid® A3WG10 BK00564 50% Glass Filled PA66 (Dry)
Overview of materials for Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Conditioned)
PBASG0459 / 132092
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.