MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ineos ABS Lustran® SAN 35  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Injection molding and extrusion grade, transparent, high gloss, improved chemical resistance, good mechanical properties.

Applications: Transparent covers, lighters, sanitary appliances, battery housings.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Key Words: Styrene-Acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
15 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 80.0 MPa11600 psi
Elongation at Break 2.0 %2.0 %
Tensile Modulus 3.70 GPa537 ksi
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm762 kV/in
Dissipation Factor 0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
Comparative Tracking Index 475 V475 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °F
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °F
Vicat Softening Point 103 °C217 °F
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 19.5 %19.5 %
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance
LG Chemical 81HF SAN Resin
Versalis KOSTIL PD C265 Styrene Acrylonitrile
Trinseo Magnum™ FG960 ABS, High Impact
Sandvik Kanthal DT Resistance Ribbon

PLANX393 / 49909

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.