MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.

Applications: Specially developed for critical applications where good chemical resistance coupled with easy identification is required. Particularly suited for the Chemical Process and Analytical Science industries. Do not use any Perlast ® grade with molten alkali metals.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070°IRHD; ASTM D1415
 7171°IRHD, +1 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 10.53 MPa1527 psi-35% change after 72 hours @ 250°C; ASTM D412
 16.2 MPa2350 psiASTM D412
Elongation at Break 154 %154 %ASTM D412
 169.4 %169.4 %10% change after 72 hours @ 250°C; ASTM D412
100% Modulus  9.59 MPa
@Strain 100 %
1390 psi
@Strain 100 %
-30% change after 72 hours @ 250°C; ASTM D412
 13.7 MPa
@Strain 100 %
1990 psi
@Strain 100 %
ASTM D412
Compression Set 35 %
@Temperature 200 °C,
Time 86400 sec
35 %
@Temperature 392 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -15.0 °C5.00 °F
Flash Point >= 400 °C>= 752 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer

PPRECI007 / 57731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.