MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Applied Composites 8022 Polyester SMC
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Industry Application: Construction
Product Application: Water Treatment
Distinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional Stability

Information provided by Applied Composites Corporation.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
Linear Mold Shrinkage 0.0012 cm/cm0.0012 in/inCold Part VS Cold Tool; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4545ASTM D2583
Tensile Strength, Ultimate 82.7 MPa12000 psiASTM D638
Tensile Modulus 10.3 GPa1500 ksiASTM D638
Flexural Strength 152 MPa22000 psiASTM D790
Flexural Modulus 8.96 GPa1300 ksiTangent; ASTM D790
 3.79 GPa
@Strain 2.5 %
550 ksi
@Strain 2.5 %
Secant; ASTM D790
 4.83 GPa
@Strain 0.5 %
700 ksi
@Strain 0.5 %
Secant; ASTM D790
Izod Impact, Notched 5.87 J/cm11.0 ft-lb/inASTM D256
Izod Impact, Unnotched 8.01 J/cm
@Temperature 23.0 °C
15.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C>= 450 °FFlexural Load; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 150 Polyester SMC
Applied Composites 120 Polyester SMC
Applied Composites 8033 Polyester SMC
Applied Composites 175 Vinylester SMC
Applied Composites 179 Polyester SMC

PAPPLI07 / 24132

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.