MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Triax® KU2-3154 ABS + Nylon 6  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,

Property data per ISO test methods.

Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³dry
Water Absorption 3.9 %3.9 %dry
Moisture Absorption at Equilibrium 1.3 %1.3 %dry
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
Calculated using room temperature density
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.0 MPa5660 psiconditioned
 55.0 MPa7980 psidry
Elongation at Break 35 %35 %Nominal, dry
Elongation at Yield 2.9 %2.9 %dry
 4.0 %4.0 %conditioned
Tensile Modulus 2.00 GPa290 ksiconditioned
 2.70 GPa392 ksidry
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²dry
 15.0 J/cm²71.4 ft-lb/in²conditioned
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
conditioned
 10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
dry
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²conditioned
 0.800 J/cm²3.81 ft-lb/in²dry
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmconditioned
 1.00e+15 ohm-cm1.00e+15 ohm-cmdry
Surface Resistance 1.00e+15 ohm1.00e+15 ohmconditioned
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
Dry
 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
conditioned
 3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
Dry
 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
conditioned
Dielectric Strength 40.0 kV/mm1020 kV/indry
 40.0 kV/mm1020 kV/inconditioned
Dissipation Factor  0.015
@Frequency 100 Hz
0.015
@Frequency 100 Hz
dry
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
dry
 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
conditioned
 0.065
@Frequency 100 Hz
0.065
@Frequency 100 Hz
conditioned
Comparative Tracking Index 600 V600 Vdry
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
36.1 µin/in-°F
@Temperature 68.0 °F
dry
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
dry
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °Fdry
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °Fdry
Vicat Softening Point 105 °C221 °Fdry
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
dry

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Lotte Advanced Materials Infino® HP-1000H PC/ABS, Unreinforced
Lotte Advanced Materials Infino® HI-1001BN PC/ABS, Unreinforced
INEOS Styrolution Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade

PLANX664 / 49979

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.