MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kennametal Stellite Stellite® 250
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.

Applications:heat treatment furnaces, metallurgical industrial furnaces such as copper smelters, baskets, grates, tray, slab skids, reheat furnaces, gas and pulverized coal burners, discharge rolls and channels, radiant tube supports, and parts in contact with molten slags and molten copper.

Corrosion: Good resistance to oxidation by air or air SO2 mixtures, and corrosive resistance by H2S up to 1249°C (2280°F). Not corroded by molten copper, but it is attacked by molten zinc and aluminum. In aqueous media, withstands attack by dilute sulfuric acid and by boiling concentrated nitric acid, but is attacked by reducing acids such as HCl.

Machinability: Has tendency to work harden, can be machined with grade C² or C³ tungsten carbide tools. A stress relief treatment of 935°C (1650°F) for 4 hours and slow cooling will aid machining.

Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc. Similar alloys include Stellite 251, Stellite 238, UMCO-50/51, Haynes 150, Esco 72

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 263263
 55
@Temperature 950 °C
55
@Temperature 1740 °F
 107
@Temperature 800 °C
107
@Temperature 1470 °F
 163
@Temperature 700 °C
163
@Temperature 1290 °F
 180
@Temperature 600 °C
180
@Temperature 1110 °F
Hardness, Knoop 271271Converted from Rockwell C hardness.
Hardness, Rockwell A 4646Converted from Rockwell C
Hardness, Rockwell B 101101Converted from Rockwell C
Hardness, Rockwell C 18 - 2918 - 29
Tensile Strength, Ultimate 551 MPa79900 psi
Tensile Strength, Yield 314 MPa45500 psi
Elongation at Break 8.0 %8.0 %
Modulus of Elasticity 217 GPa31500 ksi
Charpy Impact 36.6 J27.0 ft-lbCharpy V-notch at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.8 µm/m-°C
@Temperature 20.0 - 1000 °C
9.33 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 9.10 W/m-K63.2 BTU-in/hr-ft²-°F
Melting Point 1380 - 1395 °C2520 - 2543 °F
Solidus 1380 °C2520 °F
Liquidus 1395 °C2543 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 28 %28 %
Cobalt, Co 49.9 %49.9 %As remainder
Iron, Fe 20.5 %20.5 %
Manganese, Mn 0.75 %0.75 %
Silicon, Si 0.75 %0.75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 238 Cobalt Alloy
Kennametal Stellite Stellite® 21
Kennametal Stellite Stoody® 12 Cobalt-Base Cast Alloy
Kennametal Stellite Stellite® 251 Cobalt Alloy
Kennametal Stellite Stellite® 12

NST250 / 19209

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.