MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 770 Nickel Silver 18%, Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resistance. Typical uses include springs, resistance wire and optical goods.

Information provided by Eagle Brass Company

Key Words: UNS C77000, ASTM B122
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.69 g/cc0.314 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 76 - 8076 - 80Thickness > 0.020 Inch
Tensile Strength, Ultimate 634 - 738 MPa92000 - 107000 psi
Tensile Strength, Yield 621 - 731 MPa90000 - 106000 psi0.2% offset
Elongation at Break 3.0 - 6.0 %3.0 - 6.0 %in 2 in.
Tensile Modulus 124 GPa18000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000324 ohm-cm0.0000324 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.30 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 29.4 W/m-K204 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 55 %55 %
Nickel, Ni 18 %18 %
Zinc, Zn 27 %27 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel silver 55-18, UNS C77000, H04 Temper flat products
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
Eagle Brass 770 Nickel Silver 18%, Annealed
Eagle Brass 770 Nickel Silver 18%, Extra Spring

NEAGLE221 / 147470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.