System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ICE Al2O3 94
Categories:
Ceramic
;
Oxide
;
Aluminum Oxide
Material Notes:
Data provided by the manufacturer, International Ceramic Engineering.
Key Words:
aluminas, Al2O3, International Ceramic Engineering, aluminum oxides, ICE Al2O3 94, aluminium oxide
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
3.96
g/cc
0.143
lb/in³
Water Absorption
0.00 %
0.00 %
Mechanical Properties
Metric
English
Comments
Hardness, Mohs
9.0
9.0
Tensile Strength, Ultimate
170
MPa
24700
psi
Flexural Strength
310
MPa
45000
psi
Compressive Strength
2590
MPa
376000
psi
Fracture Toughness
4.50
MPa-m½
4.10
ksi-in½
Electrical Properties
Metric
English
Comments
Dielectric Constant
9.3
@Frequency 1e+6 Hz
9.3
@Frequency 1e+6 Hz
Dielectric Strength
9.10
kV/mm
231
kV/in
Dielectric Loss Index
0.0028
@Frequency 1e+6 Hz
0.0028
@Frequency 1e+6 Hz
Thermal Properties
Metric
English
Comments
CTE, linear
7.50
µm/m-°C
@Temperature 25.0 - 600 °C
4.17
µin/in-°F
@Temperature 77.0 - 1110 °F
Thermal Conductivity
22.4
W/m-K
155
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
1700
°C
3090
°F
Component Elements Properties
Metric
English
Comments
Al2O3
94 %
94 %
Descriptive Properties
Color
White
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al
2
O
3
Overview - Alumina, 98%, Al
2
O
3
MarkeTech Sapphire (Aluminum Oxide - Al
2
O
3
) Single Crystal
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded
CI0001 / 1377
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.