MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.5 %2.0 - 2.5 %23°C/50%RH, Starting when dry; DIN 53495
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 4.00 mm
0.0040 in/in
@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 4.00 mm
0.010 in/in
@Thickness 0.157 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi5 mm/min; ISO 527
Elongation at Break 5.0 %5.0 %5 mm/min; ISO 527
Tensile Modulus 5.50 GPa798 ksiISO 527
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °FKofler
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
 
Descriptive Properties
Back PressureLow
Holding PressureHigh
Injection SpeedMedium to High
Screw SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry
Avient Edgetek® NN-10CF/000 Nylon 6/6 - 10% Carbon Fiber
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced
EMS-Grivory Grivory® HB5299 PA*

PWELL077 / 72534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.