MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries Conduct-O-Fil® SC325P17 Silver-coated Copper Particles
Categories: Metal; Nonferrous Metal; Copper Alloy; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Applications EMI shielding, conductive adhesives, conductive paints and coatings. Advantages: Most conductive combination of metals; Dendrites give excellent compression set in FIP gaskets; Flakes make very conductive coatings; Granular particles are compatible with heat curing.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 52 µm52 µmAverage Diameter
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 17 %17 %by weight
 
Descriptive Properties
ShapeGranular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Conduct-O-Fil® SF82TF8 Silver-coated Glass Fibers
Potters Industries Spheriglass® 2429 Solid Glass Spheres
Potters Industries Conduct-O-Fil® AgClad 12 Silver-coated Glass Fibers
Potters Industries Conduct-O-Fil® S4000-S3 Silver-Coated Solid Glass Spheres
Potters Industries Conduct-O-Fil® SA270S30 Silver-coated Aluminum Granules

NPOT9976 / 161966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.