System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Toyobo T-423 Nylon, Mineral-Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
Material Notes:
Key Feature: High heat distortion and good toughness, good surface
Information provided by Toyobo Co., Ltd
Key Words:
Polyamide; Toyobo Company
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.42
g/cc
0.0513
lb/in³
ASTM D792
Water Absorption
0.67 %
0.67 %
ASTM D570
Linear Mold Shrinkage
0.0040
cm/cm
@Thickness 3.00 mm
0.0040
in/in
@Thickness 0.118 in
Linear Mold Shrinkage, Transverse
0.0045
cm/cm
@Thickness 3.00 mm
0.0045
in/in
@Thickness 0.118 in
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
120
120
ASTM D785
Tensile Strength, Ultimate
91.0
MPa
13200
psi
ASTM D638
Elongation at Break
3.2 %
3.2 %
ASTM D638
Modulus of Elasticity
6.90
GPa
1000
ksi
ASTM D638
Flexural Yield Strength
137
MPa
19900
psi
ASTM D790
Flexural Modulus
7.60
GPa
1100
ksi
ASTM D790
Compressive Yield Strength
93.0
MPa
13500
psi
ASTM D695
Izod Impact, Notched
1.20
J/cm
2.25
ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles
30
30
CS-17 wheel; ASTM D1044
Electrical Properties
Metric
English
Comments
Electrical Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
ASTM D257
Dielectric Strength
29.0
kV/mm
@Thickness 2.00 mm
737
kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance
123
sec
123
sec
ASTM D495
Thermal Properties
Metric
English
Comments
CTE, linear
45.0
µm/m-°C
@Temperature 20.0 °C
25.0
µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
210
°C
410
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
175
°C
347
°F
ASTM D648
Flammability, UL94
HB
HB
unregistered
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Toyobo GLAMIDE® T-422-02 Nylon-6
Toyobo T-422-02R Nylon, Mineral-Reinforced
Toyobo T-750 Nylon, Painting Grade
Toyobo T-400 Nylon, 15% Glass-Reinforced
Toyobo GLAMIDE® TY-791GT 6T-Nylon
PTOY47 / 70719
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.