MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.

Information provided by The Kuraray Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Brookfield Viscosity 60 cP
@Temperature 30.0 °C
60 cP
@Temperature 86.0 °F
20% wt, Toluene solution
Melt Index of Compound  0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 13 g/10 min
@Load 10.0 kg,
Temperature 200 °C
13 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 
Chemical PropertiesMetricEnglishComments
Styrene Content 20 %20 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6464ISO 48
Tensile Strength, Ultimate 8.40 MPa1220 psi
Elongation at Break 1000 %1000 %
100% Modulus 1.30 MPa
@Strain 100 %
189 psi
@Strain 100 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -14.0 °C6.80 °FDSC heating rate = -10° C/min
 
Descriptive Properties
Physical Formpellet
Viscoelasticity; Tan Delta Temp-5°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend
Kuraray HYBRAR® Low Rebound Compound # 1
Kuraray SEPTON® CM1 Compatibilizer
Kuraray SEPTON® H5127
Kuraray HYBRAR® HD2 Thermoplastic Rubber-HDPE Blend

PKUR032 / 49421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.