MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zeus ETFE Tubing and Drawn Fiber
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possesses superior toughness, stiffness and durability, all while being chemically inert. The material can be extruded in variety of forms, including flexible convoluted tubing that meets Mil Spec 81914 certification.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.70 - 1.86 g/cc0.0614 - 0.0672 lb/in³ASTM D792
Water Absorption 0.0070 %0.0070 %ASTM D257
Crystallinity 50 %50 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63 - 7263 - 72ASTM D2240
Tensile Strength, Ultimate 37.0 - 50.0 MPa5370 - 7250 psiASTM D638
Elongation at Break 200 - 550 %200 - 550 %ASTM D638
Modulus of Elasticity 0.490 - 0.780 GPa71.1 - 113 ksiASTM D638
Flexural Modulus 0.700 - 1.20 GPa102 - 174 ksiASTM D790
Coefficient of Friction 0.050 - 0.400.050 - 0.40
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.5 - 2.6
@Frequency 1e+6 Hz
2.5 - 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.7 - 70.9 kV/mm400 - 1800 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 90.0 µm/m-°C
@Temperature 20.0 °C
27.8 - 50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FASTM C177
Melting Point 230 - 282 °C446 - 540 °F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -100 °C-148 °F
Glass Transition Temp, Tg 40.0 - 80.0 °C104 - 176 °F
Decomposition Temperature 350 - 380 °C662 - 716 °FASTM E1131
Flammability, UL94 V-0V-0
Oxygen Index 30 - 46 %30 - 46 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.341.34
 
Descriptive Properties
Radiation Resistance (MRad)50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
ScanTube ETFE Tubing
Isoflon PFA Polyperfluoroalkoxyethylene
Overview of materials for Modified ETFE, Unreinforced
Zeus PEEK Tubing

PZEUS997 / 178062

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.