MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain HS Grade Optical Fused Quartz
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, inclusions, and striae, and is available in a variety of sizes and forms. It is made by electric fusion of high purity quartz powder under vacuum conditions resulting in a low [OH] (ca. 5 ppm) material.

General properties of Fused Silica and Fused quartz: A very wide transmission range from UV to near IR; extremely high optical transmission, excellent resistance to high power laser energy, excellent homogeneity, high temperature resistance, very low thermal expansion (resistance to thermal shock), and chemical inertness. General uses for optical quartz are microlithography optical systems, optical fibers, photomasks, laser optics, LCD displays, light guides, optical, IR , and UV windows, spectrophotometer cells, slides, optical pyrometers, and lamp bodies/components.

Information provided by Saint-Gobain Quartz PLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.21 g/cc0.0798 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 820820
Vickers Microhardness 1050 - 13501050 - 1350kg/m² Vickers DPH
Hardness, Mohs 7.07.0
Modulus of Elasticity 74.0 GPa10700 ksi
Flexural Strength 50.0 MPa7250 psiBending Strength
Compressive Strength 1100 MPa160000 psi
Poissons Ratio 0.170.17
Shear Modulus 31.0 GPa4500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+10 ohm-cm
@Temperature 800 °C
2.00e+10 ohm-cm
@Temperature 1470 °F
Dielectric Constant 3.78
@Frequency 100 - 2.50e+10 Hz
3.78
@Frequency 100 - 2.50e+10 Hz
Dissipation Factor  0.000060
@Frequency 1e+9 Hz
0.000060
@Frequency 1e+9 Hz
 0.00075
@Frequency 1000 Hz
0.00075
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.550 µm/m-°C
@Temperature 0.000 - 1000 °C
0.306 µin/in-°F
@Temperature 32.0 - 1830 °F
average
Specific Heat Capacity 0.750 J/g-°C0.179 BTU/lb-°F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1050 °C1920 °FNormal Conditions
 1350 °C2460 °FExtended periods if cycles remain above 300°C
 1350 °C2460 °F
 1650 °C3000 °FQuick Immersion
Softening Point 1730 °C3150 °FVaries with thermal history
Annealing Point 1140 °C2080 °FVaries with thermal history
Strain Point 1075 °C1967 °FVaries with thermal history
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.4585
@Wavelength 587.56 nm
1.4585
@Wavelength 587.56 nm
 1.4667
@Wavelength 435.83 nm
1.4667
@Wavelength 435.83 nm
ng; Temperature Coefficient = 10.6 ppm/K
Transmission, Visible >= 91 %>= 91 %Including Fresnel reflection for 10 mm pathlength
IR Transmittance  >= 85 %
@Wavelength 2600 - 2800 nm,
Thickness 10.0 mm
>= 85 %
@Wavelength 2600 - 2800 nm,
Thickness 0.394 in
Including Fresnel reflection for 10 mm path length.
 >= 92 %
@Wavelength <=2200 nm,
Thickness 10.0 mm
>= 92 %
@Wavelength <=2200 nm,
Thickness 0.394 in
Including Fresnel reflection for 10 mm path length.
UV Transmittance 90 %
@Thickness 10.0 mm,
Wavelength 270 nm
90 %
@Thickness 0.394 in,
Wavelength 270 nm
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 99.99 %>= 99.99 %
 
Descriptive Properties
Bubble Class0.1per DIN 58927
Bubbles; Sum of CSA< 0.01 mm²/100 cm³
FluorescenceBlue/Violet254 nm excitation
GranularityFaint
Residual Strain4 to 10 nm/cm
StriaeBper MIL-G-174A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fused Quartz
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Pt-10% Rh Alloy, Annealed
Pt-20% Rh Alloy, Annealed

CSTGQZ08 / 2226

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.