MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Tra-Con Tra-Pad FSBG Thermally Conductive Pad
Categories: Polymer; Thermoset; Silicone

Material Notes: TRA-PAD FSBG is a thermally conductive silicone pad. This product provides superior thermal performance. It is capable of filling small gaps, provides natural tackiness and 15% compressibility. It is designed for heat dissipation in processor and high power device applications. It has been utilized successfully to transfer heat away from an active device to a heat spreader or heat sink.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/cc
Thickness 300 microns11.8 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore C 3636
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.24.2
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 16.0 W/m-K111 BTU-in/hr-ft²-°F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Color White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Pad FSBA Thermally Conductive Pad
Tra-Con Tra-Pad FSAD Thermally Conductive Pad
Sumitomo Bakelite RX® 2-501N Diallyl Phthalate Compound
Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy
Overview of materials for Epoxy, Molded, Glass Fiber Filler

PTRAC293 / 71221

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.