MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC PP 578P Polypropylene Homopolymer for Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow properties with excellent part filling and good gloss in the products.

Typical Applications: PP 578P can be used mainly for household articles, toys and thin walled items with good dimensional stability.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 - 0.025 cm/cm0.012 - 0.025 in/in
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 36.0 MPa5220 psiASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus, 1% Secant 1510 MPa219000 psiASTM D790A
Izod Impact, Notched 0.300 J/cm0.562 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FASTM D648
Vicat Softening Point 153 °C307 °FASTM D1525B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 235 °C410 - 455 °FBarrel Temperature
Mold Temperature 15.0 - 40.0 °C59.0 - 104 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP501M Polypropylene
LyondellBasell Pro-fax HP423M Polypropylene
LyondellBasell Moplen HP550J Polypropylene
LyondellBasell Moplen EP300H Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil Exceed™ AP3AW Polypropylene Impact Copolymer

PSABICZ864 / 133060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.