MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

IDI Composites Rosite® 3550D BMC Thermoset Polyester, 20% Glass Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Key Features: Low Shrinkage

Outstanding electrical characteristics, including arc quenching. Formulated for uses with tight dimensional and warpage control and low profile for smoother surfaces

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.89 g/cc0.0683 lb/in³ASTM D792
Water Absorption 0.10 %0.10 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inshrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 36.8 - 52.8 MPa5340 - 7660 psiASTM D638
Flexural Strength 124 - 152 MPa18000 - 22000 psiASTM D790
Flexural Modulus 11.7 - 13.1 GPa1700 - 1900 ksiASTM D790
Compressive Strength 145 - 152 MPa21000 - 22000 psiASTM D695
Izod Impact, Notched 2.20 - 3.20 J/cm4.12 - 5.99 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmASTM D257
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmASTM D257
Dielectric Constant  4.8 - 5.0
@Frequency 1e+6 Hz
4.8 - 5.0
@Frequency 1e+6 Hz
ASTM D150
 5.15 - 5.35
@Frequency 60 Hz
5.15 - 5.35
@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm300 kV/inShort Time; ASTM D149
Dissipation Factor  0.010 - 0.012
@Frequency 1000 Hz
0.010 - 0.012
@Frequency 1000 Hz
ASTM D150
 0.017 - 0.019
@Frequency 1000 Hz
0.017 - 0.019
@Frequency 1000 Hz
ASTM D150
Arc Resistance 170 - 180 sec170 - 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FContinuous heat resistance; ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 760 Hybrid Adhesive Sealant
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf
3M 730 Clear Hybrid Sealant
IDI Composites Rosite® 3650D BMC Thermoset Polyester, 20% Glass Reinforced

PROS07 / 66344

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.