MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

C.O.I.M. PLAXTER® P 30 Polymeric Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description: Used for the production of extruded cables where it is requested a resistance to a temperature of 105°C.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1500 - 2000 cP
@Temperature 35.0 °C
1500 - 2000 cP
@Temperature 95.0 °F
Dynamic viscosity
 
Chemical PropertiesMetricEnglishComments
Acid Value 2.02.0mgKOH/g
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868
Tensile Strength, Yield 27.75 MPa4025 psi
Elongation at Break 266 %266 %
100% Modulus 9.20 MPa
@Strain 100 %
1330 psi
@Strain 100 %
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 3.03.0
 
Descriptive Properties
Efficiency concentration PHR32.5
N OH value (max) 20mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer
C.O.I.M. PLAXTER® P 20 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 60 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 52 Polymeric Plasticizer

PCOIM087 / 28690

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.