MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Orevac® 9314 Film EVA-MAH Terpolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: EVA Terpolymers based
Main Application: Blown film coextrusion

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Vinyl Acetate Content 13 - 14 %13 - 14 %
Melt Flow 1.5 - 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.5 - 2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 33.733.7ISO 868
Tensile Strength at Break 27.7 MPa4020 psi50 microns film; ASTM D882
Tensile Strength, Yield 5.30 MPa769 psi50 microns film; ASTM D882
Elongation at Break 570 %570 %50 microns film; ASTM D882
Modulus of Elasticity 0.0547 GPa7.93 ksiISO R527
Dart Drop Test 365 g0.805 lb50 microns film
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 °C194 °FD.S.C. method
Vicat Softening Point 70.0 °C158 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 10.2 %
@Thickness 0.0500 mm
10.2 %
@Thickness 0.00197 in
Film; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Orevac® 9304 Film EVA-MAH Terpolymer
Arkema OREVAC® 9304 EVA Terpolymer
Arkema Orevac® 18216 Maleic Anhydride modified EVA
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding

PARKG169 / 24462

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.