System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Crastin® HR5315HF BK503 PBT-IGF15
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Material Notes:
15% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.37
g/cc
0.0495
lb/in³
ISO 1183
Melt Density
1.14
g/cc
@Temperature 250 °C
0.0412
lb/in³
@Temperature 482 °F
Water Absorption
0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0050
cm/cm
0.0050
in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.011
cm/cm
0.011
in/in
ISO 294-4, 2577
Melt Flow
23
g/10 min
@Load 2.16 kg,
Temperature 250 °C
23
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
117
117
ISO 2039-2
Tensile Strength at Break
92.0
MPa
13300
psi
ISO 527-1/-2
Elongation at Break
3.4 %
3.4 %
ISO 527-1/-2
Tensile Modulus
5.20
GPa
754
ksi
ISO 527-1/-2
Flexural Modulus
4.70
GPa
682
ksi
ISO 178
Poissons Ratio
0.35
0.35
Izod Impact, Notched (ISO)
6.00
kJ/m²
@Temperature -40.0 °C
2.86
ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
10.0
kJ/m²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
@Temperature 23.0 °C
19.0
ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched
5.00
J/cm²
@Temperature 23.0 °C
23.8
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.600
J/cm²
@Temperature -30.0 °C
2.86
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
1.00
J/cm²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
IEC 62631-3-1
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 62631-3-2
Dielectric Constant
3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 62631-2-1
3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength
36.0
kV/mm
914
kV/in
IEC 60243-1
Dissipation Factor
0.0023
@Frequency 100 Hz
0.0023
@Frequency 100 Hz
IEC 62631-2-1
0.0178
@Frequency 1e+6 Hz
0.0178
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index
300
V
300
V
IEC 60112
Thermal Properties
Metric
English
Comments
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
428
°F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
ISO 75-1/-2
Glass Transition Temp, Tg
65.0
°C
149
°F
10°C/min; ISO 11357-1/-2
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
Flame Spread
32.0
mm/min
@Thickness 1.00 mm
1.26
in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index
20 %
20 %
ISO 4589-1/-2
Processing Properties
Metric
English
Comments
Melt Temperature
250
°C
482
°F
Optimum, Injection
240
-
260
°C
464
-
500
°F
Range, Injection
Mold Temperature
80.0
°C
176
°F
Optimum, Injection
30.0
-
130
°C
86.0
-
266
°F
Injection
Ejection Temperature
170
°C
338
°F
Injection
Drying Temperature
120
°C
248
°F
Injection
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.040 %
<= 0.040 %
Injection
Hold Pressure
>=
60.0
MPa
>=
8700
psi
Injection
Descriptive Properties
Back pressure
As low as possible
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
Part Marking Code
>PBT-IGF15<
ISO 11469
Polymer
PBT-I-GF15
Processing Hold Pressure Time (s/mm)
3
Injection
Resin Identification
PBT-IGF15
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
INEOS Styrolution Novodur® H604 ABS
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)
Celanese Rynite® FR530 BK507 PET-GF30FR(17)
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned)
PDSX5017 / 197657
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.