MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AURUM JCL3030 offers a unique balance of mechanical, thermal, and tribological properties for outstanding performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM components offer excellent mechanical strength and toughness, dimensional stability, low outgassing, and exceptional radiation resistance. In addition, AURUM exhibits outstanding resistance to hydraulic, automotive, and many industrial fluids and solvents, a low coefficient of thermal expansion, creep resistance, and flame retardancy. AURUM JCL3030 withstands high PV levels and provides a low wear factor and low friction surface over a broad temperature range in both dry and lubricated environments.

Applications: AURUM JCL3030 components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM parts include: thrust washers and oil seal rings for automotive and off road vehicle transmissions, thermal insulators and stripper fingers for high-speed copiers, jet engine components, check valve balls, spline couplings, heat-resistant gears, vanes, wear strips, and valve seats. Other AURUM applications include carriers for aluminum hard disks and silicon wafers, journal bearings, and bearing retainers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D792
Filler Content 30 %30 %
Water Absorption 0.23 %0.23 %24 hrs @ 73°F; ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/in
Melt Flow 27 - 37 g/10 min
@Load 10.0 kg,
Temperature 420 °C
27 - 37 g/10 min
@Load 22.0 lb,
Temperature 788 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 230 MPa33300 psiASTM D638
 141 MPa
@Temperature 149 °C
20500 psi
@Temperature 300 °F
ASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
 4.0 %
@Temperature 149 °C
4.0 %
@Temperature 300 °F
ASTM D638
Flexural Strength 314 MPa45600 psiASTM D790
 216 MPa
@Temperature 149 °C
31300 psi
@Temperature 300 °F
ASTM D790
Flexural Modulus 17.2 GPa2500 ksiASTM D790
 15.2 GPa
@Temperature 149 °C
2200 ksi
@Temperature 300 °F
ASTM D790
Compressive Strength  102 MPa
@Temperature 149 °C
14800 psi
@Temperature 300 °F
JIS K7208
 207 MPa
@Temperature 22.8 °C
30000 psi
@Temperature 73.0 °F
JIS K7208
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.94 µm/m-°C
@Temperature 20.0 °C
3.30 µin/in-°F
@Temperature 68.0 °F
MD; ASTM D696
 46.8 µm/m-°C
@Temperature 20.0 °C
26.0 µin/in-°F
@Temperature 68.0 °F
TD; ASTM D696
Melting Point 388 °C730 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 248 °C478 °FASTM D648
Glass Transition Temp, Tg 250 °C482 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
Mitsui AURUM® PL450C Polyimide
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade

PMIT045B / 53223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.