MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silres® BS 29 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® BS 29 is a water-thinnable mixture of silane, siloxane and synthetic resins. It is used in diluted form to impart both water repellency and oil repellency to inorganic substrates such as mineral construction materials. In this respect, it differs from conventional (mono-functional) water-repellents. The pores of the substrate remain open, the water vapor diffusion is hardly affected, if at all. Oil, grease, paint, etc. are easier to remove from surfaces that have been treated with SILRES® BS 29.

Application:

  • Treatment of floors of natural or synthetic stone, or unglazed ceramic tiles for easy care.
  • Treatment of window sills and table tops of natural or synthetic stone, or fibrous cement to avoid staining.
  • Treatment of facades of natural or synthetic stone, concrete, or fibrous cement in order to allow easier removal of dirt, grease, graffiti, posters, etc. from monuments, exterior and interior walls.
  • Water, oil and dirt repellent treatment of low-porosity natural stone, e. g. marble, travertine and granite.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc
@Pressure 0.1014 MPa
0.0361 lb/in³
@Pressure 14.70 psi
pH 6.06.0
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °FISO 2719
 
Processing PropertiesMetricEnglishComments
Moisture Content 70 %70 %
 
Descriptive Properties
Appearancemilky, white to yellowish
Content (%)30Silane/siloxane/polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® BS 290 Silicone Masonry Water Repellent

PWACK9532 / 205061

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.